Density (g/cm³)
Density (mg/m³)
Magnetic force, HCB (KA/M)
Magnetic force, HCB (KOE)
Magnetic force, HCJ (KA/M)
Magnetic force, HCJ (KOE)
Maximum energy (BH) MAX (MGOE)
Maximum energy (BH) MAX (kj/m³)
Molding method molding method
Remaining magnetic flux density, BR (MT)
Required magnetic field (KA/M)
Required magnetic field (KOE)
Residual magnetic flux density, br (kg)
Reverse porcelain rate, μREC
Temperature coefficient of magnetic flux density, α (%/℃)
Bending elasticity (JISK7171) (KGF/mm²)
Bending elasticity (JISK7171) MPA
Bending strength (JISK7171) (kgf/mm²)
Bending strength (JISK7171) MPA
Electrical resistance (JISC2525) μΩ / CM
Electrical resistance (JISC2525) μΩ / M
Heat expansion coefficient (JISK7179) (30-100 ° C) 10⁻⁶/℃
Pressure ring intensity (JISZ2507) MPA
Pressure ring intensity (jisz2507) (kgf/mm²)
Hardness (JISK7202) HRM
Tensile elasticity (JISK7113) (kgf/mm)
Tensile elasticity (JISK7113) MPA
Tensile strength (JISK7113) (KGF/mm)
Tensile strength (JISK7113) MPA
Part Number
NPI-6SRHandling Company
Daido ElectronicsCategories
Image | Price (excluding tax) | Bending elasticity (JISK7171) (KGF/mm²) () | Bending elasticity (JISK7171) MPA () | Bending strength (JISK7171) (kgf/mm²) () | Bending strength (JISK7171) MPA () | Density (g/cm³) () | Density (mg/m³) () | Electrical resistance (JISC2525) μΩ / CM () | Electrical resistance (JISC2525) μΩ / M () | Hardness (JISK7202) HRM () | Heat expansion coefficient (JISK7179) (30-100 ° C) 10⁻⁶/℃ () | Magnetic force, HCB (KA/M) () | Magnetic force, HCB (KOE) () | Magnetic force, HCJ (KA/M) () | Magnetic force, HCJ (KOE) () | Maximum energy (BH) MAX (MGOE) () | Maximum energy (BH) MAX (kj/m³) () | Molding method molding method () | Pressure ring intensity (JISZ2507) MPA () | Pressure ring intensity (jisz2507) (kgf/mm²) () | Remaining magnetic flux density, BR (MT) () | Required magnetic field (KA/M) () | Required magnetic field (KOE) () | Residual magnetic flux density, br (kg) () | Reverse porcelain rate, μREC () | Temperature coefficient of magnetic flux density, α (%/℃) () | Tensile elasticity (JISK7113) (kgf/mm) () | Tensile elasticity (JISK7113) MPA () | Tensile strength (JISK7113) (KGF/mm) () | Tensile strength (JISK7113) MPA () |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
![]() |
Available upon quote | 2,470 | 24,200 | 7.2 | 71 | 5.5-6.0 | 5.5-6.0 | 13,000 | 130 | 107 | 21 | 310-374 | 3.9 to 4.7 | 835-1,075 | 10.5-13.5 | 4.6-5.6 | 37-45 | injection molding | 50 | 5.1 | 460-520 | ≧ 1,592 | ≧ 20 | 4.6-5.2 | 1.13 | -0.13 | 2,550 | 25,000 | 3.4 | 33 |