Image | Part Number | Price (excluding tax) | Crystal structure | Permeation range | density | Thermal conductivity | specific heat | Young rate (e) | Poisson ratio | Band cap | Bulk absorption coefficient (10.6um) | Uniformity of refractive index (632.8nm) | foam | purity | Crystal lattice constant | Thermal diffusion |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
![]() |
ZNS |
Available upon quote |
Akira Akira (2H) |
0.36 ~ 12.0um (T = 6.0mm) |
4.09gm/cm³ |
0.272 (20 ℃ -w/cm/℃) |
0.525 (J/G/℃) |
82.0GPA |
0.270um |
3.6EV |
<0.15cm⁻¹ |
<5ppm |
none |
100.00% |
A = 3.814, C = 6.258 |
1.3x10⁻⁵ (m²s⁻¹) |