130℃/1 hour heat shrinkage <3%

150℃/1 hour heat shrinkage <5%

Air permeability

Humidity Moisture/ppm

See all 6 models in list
  • Part Number

    Boehmite coating (2u on one side)

Share this product


170+ people viewing

Last viewed: 9 hours ago


Free
Get started with our free quotation service - no cost, no obligation.

No Phone Required
We respect your privacy. You can receive quotes without sharing your phone number.

Lithium ion battery materials Ceramic coating film Boehmite coating (2u on one side)'s performance table

Image Price (excluding tax) 130℃/1 hour heat shrinkage <3% 150℃/1 hour heat shrinkage <5% Air permeability Humidity Moisture/ppm
Lithium ion battery materials Ceramic coating film-Part Number-Boehmite coating (2u on one side) Available upon quote Y Low heat shrinkage: Y ~20 seconds General: 300~500 Low heat shrinkage: 800~1,100 Resistance to humidity and heat: 400~700

There are 6 models for this product.

Customers who viewed this product also viewed

Reviews shown here are reviews of companies.

See More Ceramic Coatings Products

Other products of Toyominato Co., Ltd.

Reviews shown here are reviews of companies.


View more products of Toyominato Co., Ltd.

About Company Handling This Product

Response Rate

100.0%


Response Time

17.2hrs

  • Japan

Category of this product

This is the version of our website addressed to speakers of English in the United States. If you are a resident of another country, please select the appropriate version of Metoree for your country in the drop-down menu.

Copyright © 2025 Metoree