Engineering ceramic zirconia (ZrO2)Handling Company
Shimizu Shokai Co., Ltd.Categories
Image | Part Number | Price (excluding tax) | Dielectric constant 3GHz | Dielectric constant 1MHz | Dissipation factor 3GHz ( ×10^-4) | Dissipation factor 1MHz ( ×10^-4) | Color | Thermal shock resistance (℃) | Linear expansion coefficient RT~800℃ | Linear expansion coefficient RT~600℃ | Linear expansion coefficient RT~200℃ ( ×10^-6/℃) | Dielectric strength (kV/mm) | Hardness (HV) (Gpa) | Fracture toughness (Mpa・m1/2) | Thermal conductivity 20℃ ( W/ ( m・K) ) | Specific heat RT ( J/ ( kg・K) ) | Maximum operating temperature Oxidizing atmosphere (℃) | Bending strength 20° (Mpa) | Bulk density ( g/cm3) | Water absorption rate (%) | Volume resistivity 20℃ (Ω・cm) | Main component | Young's modulus (Gpa) | Poisson's ratio |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Zirconia (ZrO2) |
Available upon quote |
40 |
35 |
10 |
20 |
White |
280 |
11 |
10 |
10 |
10 |
13 |
6 |
3 |
470 |
800 |
1,000 |
6 |
0 |
>10^12 |
ZrO2 |
210 |
0.32 |
Reviews shown here are reviews of companies.
Reviews shown here are reviews of companies.