Cement-based crack repair material H2 Crack MaintenanceHandling Company
Hakuyu Co., Ltd.Categories
Image | Part Number | Price (excluding tax) | Test data Water binder ratio | Test data Compressive strength 7 days | Test data Compressive strength 10 days | Test data Flow value (diameter 5 x 10 cm container) | Test data Slurry density |
---|---|---|---|---|---|---|---|
H2 crack maintenance |
Available upon quote |
35.0% (test value 20℃) |
36.7N/mm2 (Test value 20℃, compliant with JSCE-G531) |
74.8N/mm2 (Test value 20℃, compliant with JSCE-G531) |
324mm (Test value 20℃, compliant with JASS 15M-103) |
1.95g/cm2 (Test value 20℃, based on JIS A 1132) |